brj-22666	Pei, Pei; Zou, Rui; Wang, Xinyao; Liu, Jinyan; Liu, Lulu; Deng, Xiaoyu; Li , Xuehua; Yu, Menghui; Tan, Jia; Li , Shizhong	Biocomposite Optimization with NaOH-modified Bagasse Fiber, Polybutylene Succinate, and Poly(Lactic Acid) using RSM Approach	2023	20	.pdf	application/pdf	7883	386	51	Initially, treated bagasse fiber was modified with KH-560 solution (silane coupling agent) and oven-dried at 80 °C. This result was associated with the suitability of treated bagasse fiber in polymer matrix with removing part of lignocellulosic components, increasing the contact area, better adhesion, and accessibility (Bartos et al. 2020; Chougan et al. 2020).	cache/brj-22666.pdf	txt/brj-22666.txt