brj-22771	Žiūra, Kęstutis; Zvicevičius, Egidijus; Černiauskienė, Živilė; Tilvikienė, Vita; Bakšinskaitė, Aušra; Pilipavičius, Jurgis	Effect of Thermochemical Treatment on the Physicochemical Properties of Fiber Hemp (Cannabis sativa L.) by-Product	2023	22	.pdf	application/pdf	11136	491	55	Compared to the raw material, the carbon content of fiber hemp stem biochar increased 1.82 times, from 45.0 ± 2.26% to 81.9 ± 8.46%, and seed husk biochar increased 1.20 times, from 56.5 ± 11.6% to 67.9 ± 7.47%. High temperature treatment increased the ash content of fiber hemp seed husk biochar by 3.49 times, from 2.08 ± 0.1% to 7.25 ± 0.2% and fiber hemp stem biochar by 3.83 times, from 2.78 ± 0.1% to 10.66 ± 0.5%.	cache/brj-22771.pdf	txt/brj-22771.txt