id	author	title	date	pages	extension	mime	words	sentence	flesch	summary	cache	txt
brj-23625	Pei, Yanghua; Xu, Yongjian; Zhang, Ying; Xu, Yang; Chen, Hao; Chen, Xin	Structure and Chemical Composition of Low-silicon White Mud Based on Technology of Black Liquor Combustion Desilication	2024	13	.pdf	application/pdf	4807	242	57	The slightly larger average particle size of LSWM compared to WM blank sample may be attributed to the adsorption of desilication agent on the surface of WM particles after the desilication process. These CaSiO3 particles are likely washed off during the washing process, resulting in an increase in WM particle size after desilication.	cache/brj-23625.pdf	txt/brj-23625.txt