cet-1483		cet-1483		6	.pdf	application/pdf	4116	169	53	In addition, at low catalyst weight loading sample, RH-2 (1:0.05), the mass loss of hemicellulose and cellulose start to decreases to 48.00 % from 48.67 % (RH- 1). 2.3 Pyrolysis experimental procedure TGA was used to investigate the weight loss of catalytic rice husk and the evolution of pyrolysis vapour simultaneously.	cache/cet-1483.pdf	txt/cet-1483.txt