id	author	title	date	pages	extension	mime	words	sentence	flesch	summary	cache	txt
mkg-1767	Ernani, Ernani; Abidin, Tri Murni; Indra, Indra	Experimental comparative study and fracture resistance simulation with irrigation solution of 0.2% chitosan, 2.5% NaOCl and 17% EDTA	2015	5	.pdf	application/pdf	4043	188	53	results The result of fracture resistance test showed the differences of fracture stress in N for each treatment group. Chitosan liquid in hydrochloric acid produces dentin surface without the smear layer and contains collagen fiber6 while Silva et al. showed that 0.2 % of chitosan is able to lift the smear layer compared to 15% of eDTA and 10% of citric acid.6 Chitosan solution has a chelating properties which cause erosion of the dentine, yet it safe for intertubular dentin.4 Mechanical destructive tests such as fracture test is important to analyze the nature of biomechanics and dental restorative materials that will be studied when given the heavy load.	cache/mkg-1767.pdf	txt/mkg-1767.txt