id	author	title	date	pages	extension	mime	words	sentence	flesch	summary	cache	txt
mkg-852	Salim, Sherman	The difference of acrylic resin residual monomer levels with various polymerization method	2011	4	.pdf	application/pdf	3080	152	51	The results of LSD test on the residual monomer levels of acrylic resin processed by different polymerization methods (mg/l) Polymerization methods Polymerization with JIS method Polymerization at 70° C for 24 hours Polymerization with microwave Polymerization with JIS method - * * Polymerization at 70o C for 24 hours - * Polymerization with microwave - Note: *: Significant 199Salim: The difference of acrylic resin residual monomer levels residual monomer that remains in the acrylic resin denture base will adversely affect the mechanical properties since the residual monomer acts as plasticizer that makes acrylic resin denture base soft and flexible.12 Moreover, the residual methyl methacrylate monomer can also come out into the surrounding tissues13 which later may cause side effects, such as the hypersensitivity of oral tissue and the changing of color stability.14 The difference of acrylic resin residual monomer levels with various polymerization method Sherman Salim Department of Prosthodontics Faculty of Dentistry, Airlangga University Surabaya - Indonesia abstract Background: After polymerization process, heat cured acrylic resin denture base actually still contains residual monomers that can become potential irritants later in oral cavity.	cache/mkg-852.pdf	txt/mkg-852.txt