id	author	title	date	pages	extension	mime	words	sentence	flesch	summary	cache	txt
eurjchem-826	Siddiqa, Asima; Sabir, Sumbul; Hussain, Syed Tajammul; Muhammad, Bakhtiar	Highly active mesoporous SiO2-TiO2 based nanocomposites for photocatalytic degradation of textile dyes and phenol	2013	8	.pdf	application/pdf	5362	296	54	No Catalyst Particle size (nm) EDX (Atomic percent) RBS (Atomic percent) TiO2 SiO2 TiO2 SiO2 1 20% SiO2‐TiO2 28 82.86 17.1 80.16 19.84 2 30% SiO2‐TiO2 25 71.53 29.3 69.23 30.77 3 40% SiO2‐TiO2 20 61.10 38.9 59.51 40.49 4 50% SiO2‐TiO2 18 48.00 52.0 51.25 48.75 XRD patterns of synthesized nanocomposite with varying SiO2 contents (20%, 30%, 40% and 50%), calcined at 550 °C are presented in Figure 1. XRD patterns of all samples and the corresponding characteristic 2θ values of the diffraction peaks confirmed the anatase‐phase of TiO2 (ICDD PDF 21‐1272). (D) Figure 9. Kinetics of adsorption of (A) auramine (B) methyl yellow, (C) phenol and (D) turquoise blue on SiO2‐TiO2 nanocomposite where, a) 20% SiO2‐TiO2 (b) 30% SiO2‐TiO2 (c) 40% SiO2‐TiO2 and (d) 50% SiO2‐TiO2 nanocomposite.	cache/eurjchem-826.pdf	txt/eurjchem-826.txt