fis-1483	Simpson, C.; Withers, P.J.; Lowe, T.; Roy, S.; Wanner, A.	Damage evolution in freeze cast metal/ceramic composites exhibiting lamellar microstructures	2015	9	.pdf	application/pdf	4432	218	56	The white circles correspond to the development of an interfacial crack, the red circles highlight the formation and growth of a series of intra-lamellae cracks and the blue arrows indicate cracking in the metal matrix. The tracked interfacial damage also began to interact with other cracks, notably merging with intra-lamellae cracks and propagating across ceramic lamellae with greater frequency.	cache/fis-1483.pdf	txt/fis-1483.txt