id	author	title	date	pages	extension	mime	words	sentence	flesch	summary	cache	txt
fis-2288	Santus, Ciro	Initial orientation of the fretting fatigue cracks in shrink-fit connection specimens	2019	9	.pdf	application/pdf	5758	406	58	The Erdogan and Sih criterion, or Maximum Tangential Stress (MTS), was followed by them and the modelled crack orientation resulted to grow outward the contact below the fretting surface, especially for low bulk stress values, thus not in agreement with the general trend of fretting fatigue cracks. A theoretical model for the prediction of initial growth angles and sites of fretting fatigue cracks, Tribol.	cache/fis-2288.pdf	txt/fis-2288.txt