id	author	title	date	pages	extension	mime	words	sentence	flesch	summary	cache	txt
fis-5507	Raju, G. U.; Meti, Vinod Kumar V.; Nadugeri, Amitkumar R.; Siddhalingeshwar, I.G.; Umarfarooq, M. A.; Banapurmath, N.R.; Sajjan, Ashok M.; Prashanth, B. H. Maruthi	Effect of pearlite nanoclay reinforcements on the mechanical and tribological behaviour of AA7076 metal nanocomposites	2025	16	.pdf	application/pdf	6281	413	45	Nanocomposites Tensile strength from FE simulation in MPa Tensile strength from experimental results in MPa Variation in results ( %) 1 wt. % nanoclay 120.16 126.27 4.84 1.5 wt. % nanoclay 157.74 146.39 7.57 Table 3: Simulation results of samples. Figure 10: (a-b) SEM micrographs of the worn surfaces of 1 wt. % nanoclay reinforced composite and (c-d) SEM micrographs of the worn surfaces of 1.5 wt. % nanoclay reinforced composite G. U. Raju et alii., Fracture and Structural Integrity, 75 (2026) 281-296; DOI: 10.3221/IGF-ESIS.75.20 291 Figure 11: (a-b) SEM micrographs of the wear debris of 1 wt. % nanoclay reinforced composite and (c-d )	cache/fis-5507.pdf	txt/fis-5507.txt