hjic-452	Ujhidy, A.; Szabó-Bárdos, E.; Horváth, O.; Horváth, A.; Schmidt, K.	Degradation of organic pollutants in photocatalytic reactors 	2011	6	.pdf	application/pdf	4473	259	43	Figure 8: Photocatalytic degradation of oxalic acid on Degussa P25 catalyst, C0(oxalic acid) 0.8 V 0 T O C / m g dm -3 m in -1 VP P90 AE P25 D P25 M PC 500 Figure 9: Initial degradation rates of oxalic acid on different catalysts Photodegradation of formic acid in the pilot equipment In order to investigate the effect of static mixer on the rate of the photocatalytic degradation of pollutants 7·10-3 M solution of formic acid was irradiated in the presence of Degussa P25 catalyst (1 g dm-3) in the pilot equipment.	cache/hjic-452.pdf	txt/hjic-452.txt